माइक्रो क्रिस्टलीय मोम.
| Sl. No. | Characteristics | Requirement | Method of Test Reference to |
|||||
| TYPE A | TYPE B | TYPE C | TYPE D | TYPE E | Annex | (P:) of IS 1448 |
||
| 1 | Drop melting point | 65-70°C | 70-80°C | 70-80°C | 85-95°C | 85-95°C | A | [P:52] |
| 2 | Ash percent by mass, Max |
0.03 | 0.03 | 0.03 | 0.03 | 0.03 | [P: 4/Sec1] | |
| 3 | Acidity: | |||||||
| a) Organic (mg of KOH per g), Max |
0.10 | 0.10 | 0.10 | 0.10 | 0.10 | [P: 2] | ||
| b) Inorganic (mg of KOH per g), Max |
0.02 | 0.02 | 0.02 | 0.02 | 0.02 | |||
| 4 | Saponification value, Max |
1.0 | 1.0 | 1.0 | 1.0 | 1.0 | [P:55/Sec1] | |
| 5 | Oil content, percent by mass, Max |
4.0 | 4.0 | 2.0 | 1.5 | 4.0 | B of IS 4654 |
|
| 6 | Colour, ASTM, Max | 2 | 2 | 0.5 | 1 | 5 | [P: 12] | |
| 7 | Needle penetration, 1/10 mm (at 25°, 5 s, 100 g) |
10 to 25 | 20 to 35 | 25 to 35 | 2 to 10 | 2 to 10 | [P: 93] | |
| 8 | Viscosity at 100°C, mm2 /s |
10 to 18 | 15 to 20 | 15 to 20 | 15 to 20 | 15 to 20 | [P:25/Sec1] | |
| 9 | Ultraviolet (UV absorbance per centimetre path length), Max |
|||||||
| 280-289 nm | 0.15 | 0.15 | 0.15 | 0.15 | D of IS 4654 |
|||
| 290-299 nm | 0.12 | 0.12 | 0.12 | 0.12 | D of IS 4654 |
|||
| 300-359 nm | 0.08 | 0.08 | 0.08 | 0.08 | D of IS 4654 |
|||
| 360-400 nm | 0.02 | 0.02 | 0.02 | 0.02 | D of IS 4654 |
|||
| 10 | Flash point, COC, ºC, Min |
260 | 260 | 260 | 260 | [P: 69] | ||
| 11 | Odour | 0 | 0 | 0 | 0 | E of IS 4654 |
||